Thursday, October 8, 2009

Annealing a zinc wire prior to forming pellets for air rifles

A fourteen-turn coil is used to heat 3.9” (100mm) of zinc wire. The wire is placed in the coil for 5 seconds to reach the desired condition just prior to the forming process...
[more about annealing][Applications]