Annealing the end of steel wire on a woven wire mesh

A two turn oval coil is used to heat the woven wire. The woven wire is placed in the coil and heated for 15 seconds to soften a 60” (1.52m) length of the wire 3” (76.2mm) deep. The woven wire is then placed in a press brake for the bending process.